Mean grain size evaluation of tungsten- and boron-carbide composites sintered at various temperatures by ultrasonic methods Online publication date: Thu, 17-Sep-2009
by Ismail Hakki Sarpun, Vildan Ozkan, Sabri Tuncel, Ridvan Unal
International Journal of Microstructure and Materials Properties (IJMMP), Vol. 4, No. 1, 2009
Abstract: In this study, the mean grain size of different ceramic-metal composites made from tungsten carbide and boron carbide have been determined with the ultrasonic velocity technique. In addition, the electroless coating method was used to coat the tungsten carbide samples. The prepared samples were sintered at different temperatures ranging from 1200°C to 1400°C in an argon atmosphere. Powders were placed in a 30 mm diameter mould and pressed using a hydraulic press at a pressure of 200 bar. The results were compared to the mean grain size obtained from Scanning Electron Microscopy (SEM). This study shows a clear dependence of ultrasonic velocity on grain size in composites of boron carbide and tungsten carbide. Especially the temperature dependence of mean grain size for tungsten carbide composites can be seen very clearly.
Existing subscribers:
Go to Inderscience Online Journals to access the Full Text of this article.
If you are not a subscriber and you just want to read the full contents of this article, buy online access here.Complimentary Subscribers, Editors or Members of the Editorial Board of the International Journal of Microstructure and Materials Properties (IJMMP):
Login with your Inderscience username and password:
Want to subscribe?
A subscription gives you complete access to all articles in the current issue, as well as to all articles in the previous three years (where applicable). See our Orders page to subscribe.
If you still need assistance, please email subs@inderscience.com